Product Catalogue/Brochure

Film Creep Tester
Film Creep Tester

Film Creep Tester is based on our Ageing Oven EB 10-II with a digital ruler system including a line laser pointer for manually measuring the creep.

The ruler is connected to a computer and the values are fed into an Excel template which calculates the result and presents the graphs.

Standards

Comply with following standards:

  • ISO 188
  • IEC 811

Temperature Range

  • +40 °C to +200 °C

Features

  • ±0,25 °C temperature variation in time and space
  • Fixed air exchange rate and low air speed
  • Adjustable over and under temperature limits with alarm
  • Temperature indicator with sensor in the inner chamber
  • Temperature controller with 0,1 °C set point
  • Cooling channels in the casing for low surface temperature
  • Run time meter
  • Countdown timer
  • Door sensor to turn off heat and illumination when door is opened
  • 4 glass window in the door
  • Digital ruler and line laser to measure the samples connected to the computer via bluetooth
  • Controlled air flow, 14 air changes /hour
  • Window, w x h 370 x 300 mm
  • Hooks to hang 10 test pieces 25 x 100 mm
  • Measuring system with laser pointer, 0,01 mm resolution, to measure elongation, range 300 mm.
  • Software to feed the data into an Excel template. Template included. This means the data is fed into an Excel template by pressing a button on the measuring scale. The test result is then calculated by the Excel template.
  • PC computer with Win XP Pro and Office software included
  • 10 Sets of grips to attach to the test pieces, together with weights,1,3 kg and 2,3 kg
Technical Specifications of Film Creep Tester
Temperature Range +40 to +200 °C

Temp. control

40 - 100 °C

101 - 200 °C

 

±0.5°C

± 1.0 °C

Temp. variation in time: ± 0.25 °C
Temp. variation in space: ± 0.5 %
Temperature sensors: PT 100, 1/3 DIN
Air speed: <0.001 m/s
Air changes: 14 changes/hour
Useful volume: 120L
Dimensions (Internal) w x h x d: 550 x 550 x 400 mm
Dimensions (external) w x h x d: 920 x 820 x 780 mm
Dimension, window, 4 glass 370 x 300 mm
Illumination of the inner chamber: 2 x 10 W, 24 V halogen
Air changes: 14 changes/hour
Weight: 103 kg
Voltage: 110-120 /220-240V 60/50Hz
Power: 2 100 W
Standards: ISO 188, IEC 811 and other technical equivalent standards

 

For more information about Film Creep Tester, please call us at 1.877.884.8378 or Click the button below.